small amounts for procedural reasons. Due to the crosslinking reaction, reactive D3 and D4 dispersions have a significantly higher formaldehyde content than classic [...] formaldehyde emissions of up to 80%. This means that the reactive Jowacoll ® D3 and D4 dispersions are below the limit values defined in various guidelines [...] and laminate (tongue-and-groove) flooring and for veneering purposes. General D3 glue with high heat resistance. 11000 ± 2000 / 20 de en fr Jowacoll ® 103.30